Precautions for filling electrode paste

Before filling, the electrode paste should be broken into 80~100mm small pieces, so that the electrode paste can pass smoothly between the two ribs. If the particle size is too large, it is easy to cause electrode paste suspension failure

Continue Reading

Production process of electrode paste

For the manufacturers of electrode paste, the two taboos of * are electrode soft break and hard break, among which soft break is more terrible and easy to cause accidents. Hard fracture is caused by insufficient strength of electrode paste after sintering

Continue Reading

Thermal shock resistance of electrode paste

The electrode paste is used as a conductive electrode under high and ultra-high temperature conditions. The operating temperature of the electrode extending out of the copper tile of the submerged arc furnace is often about 2000 degrees