Properties: The coefficient of thermal expansion is small, the resistance coefficient is low, and the mechanical strength is high.
Introduction: petroleum coke, pitch melting tank dehydrated, melted , added in proportion kneading pot kneading , and molding calcination. It has the characteristics of low resistivity and is used as a conductive material in electric furnace equipment such as ferroalloy furnaces and calcium carbide furnaces .
Production Process
Petroleum coke, asphalt melting tank dehydrated, melted , added in proportion kneading pot kneading , and molding calcination.
Our advantage
1. An annual output of 100,000 tons, large scale, low cost, and affordable.
2. Manufacturers supply, no middlemen make the difference.
3. Excellent engineers provide technical guidance, no worries about operation.
Product index
project | unit | Airtight paste | Standard electrode paste | Chemical electrode paste | |||
number 1 | number 2 | number 2 | number 3 | ||||
Ash content ≤ | % | 4.0 | 6.0 | 7.0 | 9.0 | 11.0 | 11.0 |
Volatile matter ≤ | % | 12.0~15.5 | 12.0~15.5 | 9.5~13.5 | 11.5~15.5 | 11.5~15.5 | 11.0~15.5 |
Compressive strength ≥ | MPa | 18.0 | 17.0 | 22.0 | 21.0 | 20.0 | 18.0 |
Resistivity ≤ | μΩm | 65 | 75 | 80 | 85 | 90 | 90 |
Bulk density ≥ | g/cm³ | 1.38 | 1.38 | 1.38 | 1.38 | 1.38 | 1.38 |
Elongation | % | 5~20 | 5~20 | 5~30 | 15~40 | 15~40 | 5~25 |
Common indicators in the metallurgical industry
The company’s airtight paste index
Grade item | Ash content ≤% | Volatile content % | Compressive strength MPa≥ | Resistivity μΩm≤ | Bulk density g/cm³ | Elongation |
number 1 | 3.0 | 12-15.5 | twenty three | 65 | 1.46 | 6-20 |
number 2 | 3.0 | 12-15.5 | twenty three | 75 | 1.43 | 5-20 |
Application area
Used as a conductive material in electric furnace equipment such as ferroalloy furnaces and calcium carbide furnaces .
Package
Tons of packaging, or on-demand packaging.
Properties: The coefficient of thermal expansion is small, the resistance coefficient is low, and the mechanical strength is high.
Brief introduction: Petroleum coke and pitch are dehydrated and melted in the melting tank, then added to the kneading pot and kneaded according to the proportion, and then formed and calcined. It has the characteristics of low resistivity and is used as a conductive material in electric furnace equipment such as ferroalloy furnaces and calcium carbide furnaces .
Production Process
Petroleum coke and pitch are dehydrated and melted in a melting tank, added to a kneading pot in proportion to knead, and then shaped and calcined.
Our advantage
1. An annual output of 100,000 tons, large scale, low cost, and affordable.
2. Manufacturers supply, no middlemen make the difference.
3. Excellent engineers provide technical guidance, no worries about operation.
Product index
project | unit | Airtight paste | Standard electrode paste | Chemical electrode paste | |||
number 1 | number 2 | number 2 | number 3 | ||||
Ash content ≤ | % | 4.0 | 6.0 | 7.0 | 9.0 | 11.0 | 11.0 |
Volatile matter ≤ | % | 12.0~15.5 | 12.0~15.5 | 9.5~13.5 | 11.5~15.5 | 11.5~15.5 | 11.0~15.5 |
Compressive strength ≥ | MPa | 18.0 | 17.0 | 22.0 | 21.0 | 20.0 | 18.0 |
Resistivity ≤ | μΩm | 65 | 75 | 80 | 85 | 90 | 90 |
Bulk density ≥ | g/cm³ | 1.38 | 1.38 | 1.38 | 1.38 | 1.38 | 1.38 |
Elongation | % | 5~20 | 5~20 | 5~30 | 15~40 | 15~40 | 5~25 |
Common indicators in the metallurgical industry
The company’s airtight paste index
Grade item |
Ash content ≤% |
Volatile content % |
Compressive strength MPa≥ | Resistivity μΩm≤ |
Bulk density g/cm³ |
Elongation |
number 1 | 3.0 | 12-15.5 | twenty three | 65 | 1.46 | 6-20 |
number 2 | 3.0 | 12-15.5 | twenty three | 75 | 1.43 | 5-20 |
Application area
Used as a conductive material in electric furnace equipment such as ferroalloy furnaces and calcium carbide furnaces .
Package
Tons of packaging, or on-demand packaging.